Unlocking Ultra-stable Li5FeO4 in Air: Key Advances and Practical Demonstrations

Read the full article See related articles

Listed in

This article is not in any list yet, why not save it to one of your lists.
Log in to save this article

Abstract

Li 5 FeO 4 (LFO) holds great promise as a cathode pre-lithiation additive for enhancing the energy density of lithium-ion batteries. However, its significant air instability poses a formidable barrier to commercialization. In this study, we have developed an exceptionally effective “pitch-enabled carbon encapsulation” strategy to engineer ultra-stable LFO. By leveraging the meltability of pitch, a compact carbon coating can be formed on LFO (LFO@C), enabling it to retain a substantial capacity of 745.1 mAh/g even after 72 hours of exposure to air with 20% relative humidity (RH). Notably, this retained capacity after 72 hours constitutes 92.6% of its initial capacity and 85.9% of its theoretical maximum, representing the best air stability reported for LFO to date. In contrast, pure LFO rapidly declines to just 14.3% of its initial capacity within 4 hours under the same conditions. Beyond enhancing air stability, the carbon coating also improves LFO's specific capacity, rate capability, and cycling stability. To demonstrate its practical application, we assembled a pouch-type full cell on an industrial pilot line, accompanied by comprehensive failure analyses. The results indicate that the incorporation of LFO@C boosts the pouch cell's energy density by 13.7%. We believe that this work will significantly accelerate the real-world implementation of LFO.

Article activity feed