Effect of surface treatment on bonding strengths of hard and soft reline materials to 3D-printed denture base resin

Read the full article

Listed in

This article is not in any list yet, why not save it to one of your lists.
Log in to save this article

Abstract

To evaluate the effects of surface treatment and thermal cycling on the tensile bond strength of hard and soft reline materials to a 3D-printed denture base resin (3DP) compared with a conventional heat-polymerized resin (HC). Specimens of 3DP and HC resins received no treatment, alumina sandblasting, dichloromethane priming, or 4-META/MMA-TBB resin (4-META) application. One hard reline material (HR), two acrylic-based soft reline materials (AC1 and AC2), and one silicone-based soft reline material (SI) were evaluated. Tensile bond strength was measured after 24 h of water storage (TC0) or 5,000 thermal cycles (TC5000) ( n  = 20). A significant four-factor interaction demonstrated that bond strength depended on the denture base resin, reline material, surface treatment, and thermal-cycling condition ( P  < 0.05). The hard reline material showed significantly higher bond strength than all soft materials ( P  < 0.05). For the 3DP resin, 4-META yielded the highest bond strength for AC1 under both aging conditions ( P  < 0.05) and improved bonding of HR and AC2 relative to untreated specimens ( P  < 0.05). In contrast, the silicone-based reline material exhibited limited responsiveness to surface treatment, and thermal cycling generally reduced bond strength. Bond durability between denture base and reline materials was influenced by the interaction among resin type, reline material, surface treatment, and thermal aging. Among the evaluated surface treatments, 4-META improved bonding for acrylic-based reline materials on the tested 3DP. The surface treatment protocols should be tailored to the specific denture base–reline material combination and anticipated aging condition.

Article activity feed