In-Situ Fabrication of Ductile Ti-TiCx Metal Matrix Composite by Laser Powder Bed Fusion with Enhanced Elastic Modulus

Read the full article See related articles

Listed in

This article is not in any list yet, why not save it to one of your lists.
Log in to save this article

Abstract

The production of high stiffness Ti-based Metal Matrix Composites (Ti-MMCs) displaying significant ductility by additive manufacturing technologies is not yet at the level of conventionally produced Ti-MMCs. This study outlines the production process of stiffness-driven Ti-TiC MMCs displaying a remarkable ductility. The process consists in powder Mechanical Blending, Laser Powder Bed Fusion (LPBF), and a heat treatment. A TiC fraction of more than 20 vol% was formed in-situ through the reaction of titanium with carbon during the LPBF process. The as-built sub-stoichiometric TiC dendrites are converted in equiaxed TiC grains during the heat treatment. The TiC C/Ti ratio was found to be close to 0.5 in as-built conditions, and 0.7 in heat treated conditions, resulting in an effective reinforcement content nearly twice the one expected for stoichiometric TiC, leading to stronger reinforcement. The mechanical analysis revealed a Young’s modulus of up to 149 GPa and total elongations of up to 2.8%. The former represents a 27% improvement compared to commercially pure Titanium and the latter exceeds by 115% reported values for LPBF Ti-MMCs with similar Young’s modulus. It is enabled by the in-situ formation of defect-free TiC reinforcements combined with their globularisation through heat treatment.

Article activity feed